Leaktightness in vacuum conditions.
Test methods
A pipe and accessory assembly is subjected to a partial vacuum for a set period of time. The leaktightness of the joints is checked during the test.
Products to test
Plastics piping systems for hot and cold water in buildings made of:
Polypropylene (PP) EN ISO 15874-1, -2, -3, -5
Cross-linked polyethylene (PE-X) EN ISO 15875-1, -2, -3, -5
Polybutene (PP) EN ISO 15876-1, -2, -3, -5
Chlorinated poly (vinyl chloride) (PVC-C) EN ISO 15877-1, -2, -3, -5
Multilayer EN ISO 21003-1, -2, -3, -5
Raised temperature resistance (PE-RT) EN ISO 22391-1, -2, -3, -5